Documenting Concrete Crack and Defect Patterns

Map crack orientation and relation to supports or joints. Use the example below to practice the review and record an output that another reviewer can reproduce.

A crack crossing an exposed concrete surface
Concrete Cracked by John Harvey (public domain)

Inputs and Prerequisites

Scaled photographs, fixed stations, dated survey and an exposure record.

Review Workflow

  1. Crack map
  2. Measure width
  3. Repeat visit
  4. Interpret
  1. Map crack orientation and relation to supports or joints.
  2. Record width using a consistent measurement technique.
  3. Compare repeated measurements under similar conditions.

Worked Example

At one marked station an illustrative width changes from 0.20 mm to 0.30 mm. The observed change is 0.10 mm. If the instrument is repeatable only to about 0.10 mm, repeat before concluding that the crack is widening.

Output Checks and Common Errors

Record instrument resolution, temperature and surface condition with every reading.

Official References